Dear All,

In the latest edition of ISO 15614-1 : 2019, it is stated that, "Level 1 is based on the requirements of ASME BPVC Section IX, Welding, Brazing, and Fusing Qualifications, and Level 2, for which the extent of testing is greater, is based on the previous version of this standard; BS EN ISO 15614-1:2004+A2:2012. It is important to note that a procedure test carried out to Level 2 automatically qualifies for Level 1 requirements, but not vice-versa"

Is it possible to write a WPS as per ASME Section IX with Level 1 with a supporting PQR tested as per EN ISO 15614-1 (Level 2). 

Regards,
Sankalp

Xuân Thông

unread,
Feb 5, 2022, 2:21:46 AM2/5/22
to material...@googlegroups.com
Dear Sir,
Please refer to below paragraph 
When no level is specified in a contract or application standard, all the requirements of level 2 apply.
So that I think you can not use the PQR as per ASME IX for supporting level 2
Regards,
Bui Xuan Thong


Vào Th 6, 4 thg 2, 2022 vào lúc 10:20 S.Sankalp <sidd.s...@gmail.com> đã viết:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/816e3a9e-c37e-45f4-99fd-a90897cfa39fn%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages