TEST REQUIRED

83 views
Skip to first unread message

sujit kumar

unread,
Jun 17, 2022, 8:33:21 AM6/17/22
to Materials & Welding
Hii Experts,

hope all is well.

I want to know which test is required for WPS and how many tests are required as per ASME section IX.?

PLATE SPECIFICATION-SA516  GR70
PLATE THICKNESS-10MM
FILLER USED-ER-70S2
ELECTRODE USED-E-7018
 TOUGHNESS TEST NOT REQUIRED



Best regards
Sujit Kumar

Rameshbabu B

unread,
Jun 17, 2022, 10:23:36 AM6/17/22
to material...@googlegroups.com
Hi Sujit, 

Referring to QW-451.1 the following tests shall be conducted.

2 Transverse tensile
2 Root Bend
2 Face bend

Additionally, you can advise the laboratory to perform a hardness test for Base, Weld, and HAZ which is common when qualifying a PQR


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0d00b35e-1d18-400f-9bf6-a9a55001f9a0n%40googlegroups.com.


--

Ramesh Babu Balaram

Corporate Head, Quality

The Oriental Towers, No. 461, 1st Floor, 17th Cross Road, 4th Sector,

Sector 4, HSR Layout, Bengaluru, Karnataka 560102.

M 9840531355  E ramesh...@zetwerk.com  W zetwerk.com

App Green Footer Image Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hard copy.



This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

Kannayeram Gnanapandithan

unread,
Jun 18, 2022, 5:34:36 AM6/18/22
to materials-welding
Hardness test requirements, is it required as per code or Project specification requirements

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Rameshbabu B

unread,
Jun 19, 2022, 11:15:30 PM6/19/22
to material...@googlegroups.com
Generally while qualifying PQR following shall report

Tension
Bend 
hardness (additional)
Macro (additional)

According to project spec
Toughness test 
Hardness 
Macro 

--
Regards
Ramesh Babu Balaram
Head QA/QC
Zetwerk Manufacturing Businesses Private Limited
Mobile: +91 98 4 053 13 55

>>>DONATE NOW<<<
SUPPORT ZETWERK’S CAMPAIGN TO FEED THE VURNERABLE MIGRANT FACTORY WORKER POPULATION.
Contribute generously. Each donation will go towards essential ration kits.
Let’s come together as a nation so that they don’t have to go hungry
Reply all
Reply to author
Forward
0 new messages