Suitable filler and and electrodes

16 views
Skip to first unread message

JAYAPAL DHAKSHNAMOORTHY

unread,
May 25, 2019, 1:44:06 AM5/25/19
to material...@googlegroups.com
Dear experts,

I have to qualify the the PQR as per (ASME Sec IX 2017)  for the the following

Material: (SA516Gr.60+SB127)+(SA516Gr.60+SB127), that is SA265 Clad plate.

Process: GTAW+SMAW (Image attached below)

Groove: single "V" groove weld.

Thk.:22mm+3mm of clad.

Kindly advise the suitable filler wire and electrode.SFA no. & Classification no. 


Regards.
Dhakshnamoorthy.J

Untitled.jpg

Chintan

unread,
May 27, 2019, 12:02:15 PM5/27/19
to Materials & Welding
Use NiCu7

George Dilintas

unread,
May 29, 2019, 12:04:06 PM5/29/19
to material...@googlegroups.com
for the base metal or for the cladding?
Typical for this base metal E7018 & ER70-6, 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHHcqJcqY-zQf8FGmv4diMbYjs75YvKRnC_-U8_sxTHXX2KChg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

JAYAPAL DHAKSHNAMOORTHY

unread,
May 29, 2019, 12:04:06 PM5/29/19
to material...@googlegroups.com
For 
GTAW:ER NiCU-7
SMAW:E 7018

Anybody done this process?

On Mon, 27 May 2019, 21:32 Chintan <chin...@gmail.com wrote:
Use NiCu7

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
Reply all
Reply to author
Forward
0 new messages