Dear Experts,
Greetings!! 

Increase of Heat Input considered as an essential variable in SAW welding if impact test is required. Anybody can define the word "Increase" or how much 

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

Ahmad el-sharkawy

unread,
Sep 12, 2022, 7:14:02 AM9/12/22
to material...@googlegroups.com
Increase more than the maximum heat input in the PQR.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ71_10vgqbJU6DNuratfCoqbH1uF%3Dz3Yrhj29-Gn9PMgA%40mail.gmail.com.

Kannayeram Gnanapandithan

unread,
Sep 13, 2022, 11:34:20 PM9/13/22
to materials-welding
any increase more than PQR

--