2160 PSI - Reparing Separator 2" Nozzles

24 views
Skip to first unread message

williams p wilson

unread,
Apr 21, 2015, 4:41:14 AM4/21/15
to material...@googlegroups.com
Dear Experts,

Greetings..

Kindly advice which type of welding procedure & heat treatment for 2", Sch 160  nozzle pipe end joining with 75 mm thick carbon steel body Separator. 

Please reply with Pre heating temperature, Intervals of Heating, PWHT Procedures, Welding Rods Details


Thanks in Advance..

Williams.


Pictures attached for your reference.


Separator Pics-1.jpg
Separator Pic.2.jpg
Separator Pic.3.jpg
2 Nozzle End face.jpg

Jim Price

unread,
Apr 21, 2015, 7:56:31 AM4/21/15
to material...@googlegroups.com

Can you give more specifics on material and grade?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7fysvWYxFHv9cp%3DL%2B-gneiAU0TXosY031wXTaEjuErNg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

williams p wilson

unread,
Apr 21, 2015, 11:56:16 PM4/21/15
to material...@googlegroups.com
Dear Sir,

Greetings..  

Materials Grade -  Base Metal - P1 Gr. 1,2

Type of Weld - One side Bevel Groove and double fillet weld  

Thickness of Separator Shell Plate - 75 mm


Thank you and regards,

Williams

Mobile No. 00968-96004969