Dear Experts,
please suggest the welding consumable for the combinations of materials provided below,
1. 410S to 410S - P No. 7 to P No. 7
2. SA516 Gr. 60 with TP405 Clad to SA 240 TP 405
3. SA 240 TP 405 to SA 240 TP 405 - P No. 7 to P No. 7
4. 410S to SA 240 TP 405
Regards
Anandh Kumar