P NO - A 560 50Cr-50Ni Nb

151 views
Skip to first unread message

samaran sadasivam

unread,
Mar 27, 2016, 12:02:10 AM3/27/16
to material...@googlegroups.com
Dear Experts,

Can anyone pls to tell me what is the P No for the pipe material ASTM A560 Gr 50Cr 50Ni Nb??. 



Thanks & Regards

S.Samaran

Lalu Rajendran

unread,
Mar 27, 2016, 1:07:04 PM3/27/16
to material...@googlegroups.com
Hi,

ASTM A560 Gr 50Cr 50Ni Nb is a chromium nickel alloy casting and is not assigned to a P number. You can use ENiCr-4 electrodes. Please refer SFA 5.11 table-1.

regards,
LALU

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGxS6aSH9b34m5h_GRaD7W%2BmzpzmFsN6J9sCRZV3rU9W7%2BfK0w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages