Non Shrinkage Grouting in storage Tank before or after hydro
62 views
Skip to first unread message
jayadeep C
unread,
Jul 27, 2020, 3:33:18 AM7/27/20
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Hi,
Please advise the grouting of the storage tank may carryout before the hydrotest or after the hydro test? Here we are using Non shrinkage grouting. Apart from this any other materials are using elastomeric based vapor barrier sealant?