Required sample copy of welding procedure Specification for Galvanized pipe welding..

132 views
Skip to first unread message

HARISH VARUDE

unread,
Apr 14, 2021, 11:42:00 PM4/14/21
to material...@googlegroups.com
Respected experts,

If any have sample copy of approved welding procedure with PQR for Galvanized pipe welding.please share me for reference..

From
Herish varude
Mob.No.:-7990746918

Vishwas Keskar Welding Manager WELDING

unread,
Apr 15, 2021, 12:08:13 AM4/15/21
to Materials & Welding
The WPS is same   in line with ASME SEC IX.

The  consumable is E6010 as welding is to be done on Galvanized parts 

pgos...@rogers.com

unread,
Apr 15, 2021, 12:10:23 AM4/15/21
to material...@googlegroups.com

Galvanized steels are zinc coated carbon steels(typically). Zinc removal prior to welding is advisable, as Zinc creates lot of fumes, plus Zinc deposition is done under acidic solutions, which may cause dissolution of hydrogen. Attached is the article which explains how to handle such steels and successfully welding them. Additionally, you may download this AWS standard so as to find the necessary resources for welding Galvanized steels.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of HARISH VARUDE
Sent: April 14, 2021 8:09 PM
To: material...@googlegroups.com
Subject: [MW:32247] Required sample copy of welding procedure Specification for Galvanized pipe welding..

 

Respected experts,

 

If any have sample copy of approved welding procedure with PQR for Galvanized pipe welding. Please share me for reference..

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKKH_q2-DUfdTQ9T6T%2BOXSjAveADRzdhM8ci4MSugA%2B6xw%40mail.gmail.com.


Virus-free. www.avg.com
Guidelines for Welding Galvanized Steel.pdf
WZC-D19.0-72PV (1).pdf