Re: WPS qualified in 5G and Welder qualification required in 6G

135 views
Skip to first unread message

HARISH VARUDE

unread,
Jul 20, 2020, 1:05:37 AM7/20/20
to material...@googlegroups.com
As API 1104 specifications

From
Herish varude
Mob.No.:-7990746918

On Mon, Jul 20, 2020, 10:17 AM HARISH VARUDE <harish....@gmail.com> wrote:
Dear all,

Contractor have a Approved WPS in 5G position and now he want to do weld joints in 2G position and also want to welder qualification in 6G position.
Can it possible???

From
Herish varude
Mob.No.:-7990746918

HARISH VARUDE

unread,
Jul 20, 2020, 1:05:48 AM7/20/20
to material...@googlegroups.com

Sandeep Pr

unread,
Jul 20, 2020, 1:41:45 AM7/20/20
to material...@googlegroups.com
Dear Brother,

As per API 1104, Rolled to Fixed or Vice Versa require Requalification.for Procedure.

Hence WPS Does not Qualifies for 2G Position.

But WPS do qualify 6G Position. Hence Welder qualificaton can be done in 6G Position.

Please Find the screenshot of the Same

image.png

Hnce 
With Regards,

Sandeep.P.Raghavan


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YK%2B69MY7CMiRy1yKR2gKcD%2B-W4r%2B1RCNBU%3DNvZ%3D6simwHw%40mail.gmail.com.

HARISH VARUDE

unread,
Jul 20, 2020, 1:58:08 AM7/20/20
to material...@googlegroups.com
Thank you,

I have already instructed to contractor for re qualification / new WPS in 6G position...