Dear Sirs,
Presently we are doing hot dip galvanization of pipe spools where we
have to protect the serration of flanges during galvanization.

Can any body suggest what can be applied on serration to protect it
from adhesion of ZINC on serration.

Please Advise.

Regards
Arvind

mazlan abd aziz

unread,
Mar 31, 2015, 11:07:23 PM3/31/15
to material...@googlegroups.com
Just apply silicon gel on the flange face , this is what they did in the galvanizing plant.

Best Regards


Mazlan Abd Aziz
Freelance inspector

On Mon, Mar 30, 2015 at 5:49 PM, senthil aravind <k.senthi...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (k.senthi...@gmail.com) Add cleanup rule | More info
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABsdp%3Dhxthn0ujzS3ckEkLa%2Bne7a-EGZQS8twYujryySuz4CSw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages