how to calculate hydrostatic head

73 views
Skip to first unread message

smkabeer ahamed

unread,
Feb 23, 2016, 1:47:45 AM2/23/16
to Materials & Welding
Dear sirs,

How to calculate hydrostatic head during hydrostatic test

Mohammed Ghani

unread,
Feb 23, 2016, 5:21:31 AM2/23/16
to material...@googlegroups.com
0.49 PSI / Sq feet elevation

On Tue, Feb 23, 2016 at 9:23 AM, smkabeer ahamed <sm_kabe...@yahoo.co.in> wrote:
Dear sirs,

How to calculate hydrostatic head during hydrostatic test

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1930655751.6911038.1456208608393.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

Kunal Patel

unread,
Aug 1, 2016, 1:24:22 AM8/1/16
to Materials & Welding
P=qgh
P=pressure
q= densiry of water 1000kg/m3
g= 9.81m/s2
H=head suppose 10 m

P= 98100N/m2
P=1.013kg/cm2

Where 1 N= 1 kg.m/s2


Hence @ 10 m height we consider pressure 1 kg/cm2.

Regards
Kunal Patel