Dear Expert,

We want submit pressure test to Client, please advise to me about How much maximum pressure drop / down which allowable in pressure test at site?

Thanks & Regards
Winarko

Mohd Siraj

unread,
Nov 15, 2015, 12:17:10 AM11/15/15
to Materials & Welding
you are doing inservice hydro test refer API570.

Mohammed Ghani

unread,
Nov 15, 2015, 12:17:25 AM11/15/15
to material...@googlegroups.com

Dear,

Be specific on type of pressure test..
Is it a hydrostatic,  pneumatic or RF PAD pressure test..?
Is it for a vessel or boiler?
Is this new or in service equipment?

Let us know this details to guide you further

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMoAFwoXWjUG76i9aNq8aKDBjPg%2BWS_B8%2BmPVzTbMY8JieBURg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Mohammed Ghani

unread,
Nov 15, 2015, 1:29:27 AM11/15/15
to material...@googlegroups.com
Dear,

If it is a piping pressure test refer API 570,
If Vessels pressure test Refer API 510.

Regards

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMoAFwoXWjUG76i9aNq8aKDBjPg%2BWS_B8%2BmPVzTbMY8JieBURg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

Reply all
Reply to author
Forward
0 new messages