pipeline crossing highway

163 views
Skip to first unread message

QA/QC

unread,
Nov 11, 2020, 5:19:07 AM11/11/20
to Materials & Welding
Dear experts 

we are going to erect a new pipleline crossing a principal road with many cars and track of big load so what  we can do to protect our pipe from big load anything from code and standards 

can u help me 

sajeed zaheer

unread,
Nov 11, 2020, 6:12:19 AM11/11/20
to material...@googlegroups.com
Go through ASME 31.8 for gas transmission distribution piping system 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4d25efc3-f435-4b4a-bb71-74d29665bf0bn%40googlegroups.com.

Leonardo Gracia

unread,
Nov 11, 2020, 6:40:57 AM11/11/20
to material...@googlegroups.com

API RP 1102 Steel Pipelines Crossing Railroads and Highways

Adnan Ziad

unread,
Nov 11, 2020, 8:49:36 AM11/11/20
to material...@googlegroups.com
whats the procedure to do can anyone mention it to me please 

pgos...@rogers.com

unread,
Nov 11, 2020, 4:13:54 PM11/11/20
to material...@googlegroups.com

Hi,

You need to take a look at this document. Chapter-7 outlines the guidelines about  pipelines crossing highways.

 

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

Pages from API 1102 2017.pdf

Tom Lee

unread,
Nov 11, 2020, 10:45:37 PM11/11/20
to material...@googlegroups.com
Adnan,

You might look into spray Polyurethane foams of high density.  The foam has been used on pipelines as support, and be layered above the pipe (and below) to give you the support you need.

Tom Lee