HARDNESS TEST

46 views
Skip to first unread message

Elavarasan Mech

unread,
May 23, 2025, 8:42:14 AM5/23/25
to material...@googlegroups.com
Dear all
 
API6A FLANGE which hardness method recommended please guide me
Regard 
ELAVARASAN 

Deerendra Karanth

unread,
May 23, 2025, 1:09:50 PM5/23/25
to material...@googlegroups.com
Sir, 

Use Brinell or Rockwell C as per the heat treatment and material type.The test location, frequency, and acceptance criteria must comply with API 6A PSL level (usually PSL 2/3) and material class (AA, BB, CC...).

BR 
Deerendra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ykHf%3D_jc7zpJqgC1GYN4UkJ_aMLroy0YsnLNY2TO5oCNQ%40mail.gmail.com.

George Dilintas

unread,
May 26, 2025, 5:32:34 AM5/26/25
to material...@googlegroups.com
The standards referenced in API 6A are all for Brinell hardness testing
Δρ. Γεώργιος Διλιντάς
Ηπείρου 5 , Μελίσσια - 15127
Αεροναυπηγος Μηχανικός - Μελος ΤΕΕ 55018
Τηλ +30 210 8100578, +30 6944 646 204

Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I,  Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis


Reply all
Reply to author
Forward
0 new messages