Dear All
  as per ASME SEC II PART C in the welding rod MTC lot class & schedule (LEVEL OF TESTING) specified in the certificates mandatory or not, please guide me.  

Regards 
ELAVARASAN

Deerendra Karanth

unread,
May 13, 2025, 10:22:55 PM5/13/25
to material...@googlegroups.com

Mandatory testings must be done per the SFA specification (Lot Class & Schedule).

BR,
Deerendra


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4yko6W8yj8CWpenRLXqh89%3D-yktdFFd0f-ybtXPVBYpHJA%40mail.gmail.com.

Elavarasan Mech

unread,
May 14, 2025, 2:53:22 AM5/14/25
to material...@googlegroups.com

Above attached MTC acceptable or not pleaee guide me




Deerendra Karanth

unread,
May 14, 2025, 6:10:28 AM5/14/25
to material...@googlegroups.com

MTC appears acceptable; however, kindly confirm if end user specifications or applicable WPS/PQR require any supplementary tests such as impact toughness, intergranular corrosion (IGC), or hardness. All other parameters are in line with Sec II C requirement.

BR

Deerendra 