   Good day. Can any expert give me a reference for Piping joint can't  rest of Pipe Support or any part of structure?? Is there any International standard cover this topic ??

Deerendra Karanth

unread,
Feb 25, 2025, 12:30:55 PM2/25/25
to material...@googlegroups.com

As per international standards:

ASME B31.3 (Clause 321.1.2, 321.1.3) – Piping joints should not rest on supports to prevent undue stress and allow inspection.

ASME B31.1 (Clause 114.3, 120.1) – Supports must not interfere with expansion or place stress on joints.

API 570 – Ensures accessibility for inspection and maintenance.

MSS SP-58 – Recommends support placement away from joints.

Regards
Deerendra


On Tue, 25 Feb, 2025, 21:09 Mudssar Raza, <mudassar...@gmail.com> wrote:
Hy,
   Good day. Can any expert give me a reference for Piping joint can't  rest of Pipe Support or any part of structure?? Is there any International standard cover this topic ??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/434d282d-2951-4d30-bab7-94c92e45bb51n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages