Hardox to Hardox Butt welding joints

45 views
Skip to first unread message

VHEER RAJHU

unread,
Jul 30, 2015, 2:07:09 AM7/30/15
to materials-welding
Dear Experts,

We need to do butt welding of Hardox 400 Plates thk 20mm for one of our projects. Could any body suggest me which electrode  to be used.

Best Regards

Vheerrajhu

Kannayeram Gnanapandithan

unread,
Jul 30, 2015, 4:47:34 AM7/30/15
to materials-welding
7018-1/8018

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFz2VvT2S3R-cqOz7R-pg1M78n7jYNExJ%2BC-cAL%2BznW0HDG-Cw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

pgoswami

unread,
Jul 30, 2015, 6:37:27 AM7/30/15
to material...@googlegroups.com
Hi Vheerrajhu,
 
Please see the link below for more details and guidelines.
 
Thanks.
 
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 
http://www.winfa.sk/pdf/wel.pdf

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Kannayeram Gnanapandithan
Sent: Thursday, July 30, 2015 4:45 AM
To: materials-welding
Subject: Re: [MW:23231] Hardox to Hardox Butt welding joints

Kunal Patel

unread,
Jul 30, 2015, 7:29:52 AM7/30/15
to Materials & Welding, rajuve...@gmail.com
Dear friend,

Pl. find attachment. It may help you.

regards,
Kunal-BVIS
Welding HARDOX and WELDOX[1].pdf