Tests as per AWS D 1.1 for buttering

112 views
Skip to first unread message

prashant pansare

unread,
Nov 15, 2015, 1:47:42 AM11/15/15
to mat wel
Dear All,

As per AWS D 1.1 Clause No 5.22.4.3 correction is allowed in root openings.

1) Shall we conduct  WPS for buttering?
2) What tests to be carried out to qualify the WPS?

--
Thanks & Regds,

Prashant  Pansare
Cell no - 09987189854