Dear expert 
What is the filler wire for below mentioned mention Material

1. FILLER WIRE FOR HASTELLOY B TO HASTELLOY B  BASE MATERIAL WELDING

2.FILLER WIRE FOR DUPLEX TO DUPLEX BASE MATERIAL WELDING

3. FILLER WIRE FOR ENCONEL 602 TO SS 316 BASE MATERIAL WELDING 


Best regards
Sujit kumar

wi...@shantimetal.com

unread,
Dec 17, 2022, 9:44:55 AM12/17/22
to Materials & Welding
ERNIMO10