SS304 TO SS304H
37 views
Skip to first unread message
sujit kumar
unread,
Sep 13, 2022, 11:34:15 PM
9/13/22
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Dear all,
I am having ss 304 to ss 304 Qualified WPS. can I use the same QPR to Qualify SS304 to SS304H and what filler wire we should use?