Dear Experts,
ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding?
Thanks,
Pkm.
| From: Raghuram Bathula Sent: Saturday, 17 January 2015 18:23 To: Materials-Welding Reply To: material...@googlegroups.com Subject: Re: [MW:22729] ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding? |
4.2.2.1, Previous Performance Qualification. Previous performance qualification tests of welders, welding operators, and tack welders that are properly documented are acceptable with the approval of the Engineer. The acceptability of performance qualification to other standards is the Engineer's responsibility, to be exercised based upon the specific structure, or service conditions, or both.
| From: Harikrishnan N S Sent: Thursday, 22 January 2015 10:35 Reply To: material...@googlegroups.com Subject: [MW:22742] Re: ASME Sec IX Piping Qualified welders can possible to AWS D 1.1structural welding? |