What will be the thickness requirement for PWHT of Branch Weld(O-Let) and Support direct welded to the pipe.
ASME B 31.3 clause 331.1.3 says
When components are joined by welding, the thickness to be used in applying the heat treatment provisions of Table 331.1.1 shall be that of the thicker component measured at the
joint, except as follows:
a) (a) In the case of branch connections, metal (other than weld metal) added as reinforcement, whether an integral part of a branch fitting or attached as a reinforcing pad or saddle, shall not be considered in determining heat treatment requirements.

If i am adding reinforcement pad / Cradle support > 20mm thick directly welded to the run pipe, is it required PWHT regardless of material or service?


Heat treatment is required, however, when the thickness through the weld in any plane through the branch is greater than twice the minimum material thickness requiring heat treatment, even though the thickness of the components at the joint is less than the minimum thickness.

If i have a 20mm thick pipe and i am welding one O-let we have a weld size maximum 30 mm. Did i need PWHT on the case?  or if the weld size is 40 mm then only i need to do the PWHT?

 I am just confused to get the actual Pipe thickness required for PWHT for Branch Connection (Pipe-Pipe, Pipe - Olet) and also for support-pipe welding. I need this reagrdless of material and service.

Can you please clarify.
I will be helpful with your valuable comment.

--
Thanks & Regards
Biplab Pal
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

george....@gr.bureauveritas.com

unread,
May 4, 2015, 8:11:24 AM5/4/15
to material...@googlegroups.com, Abhilash Krishnan, Pinaki Boxi, Chandan Majumdar

your pipe is 20 mm and supposing your material Pno is 1, the weld metal analysis is 1 also.
You are on the limits, so if the other pipe (main) has a thickness 20 mm max you do not need any PWHT.
If your weld thickness (through any plane) is larger than 40 mm, then you have to apply PWHT.
The thickness of the reinforcement does not count, but if the thickness of the weld attaching the reinforcement to the pipe together with the thickness of the weld attaching the branch is larger than 40 mm then you need PWHT

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Biplab Pal ---04/05/2015 14:35:45---Dear Experts, What will be the thickness requirement for PWHT of Biplab Pal ---04/05/2015 14:35:45---Dear Experts, What will be the thickness requirement for PWHT of Branch Weld(O-Let) and

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAFnzQg1%2BfeOMmcBi3W7FTMoEgEHNAHA68%2BYZOfNY7Sgot2ohhw%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Reply all
Reply to author
Forward
0 new messages