Dear All,
We are having a FCC unit where "Ultimet alloy-1233" is used in scrubber nozzles. It is observed severely eroded from the internal and external surface. It is presently having a pump volute design with casting.

Request to kindly guide on how to carry out weld build-up/ application of overlay patch on such cobalt rich metallurgy.

It is possible to provide a case hardened material for such high erosive applications? 

Regards,
Devang Majithia

pgos...@rogers.com

unread,
Jul 14, 2020, 5:11:18 PM7/14/20
to material...@googlegroups.com

Hi

This alloy is difficult to repair. The eroded area should be uniformly ground and made free of cracks first.

Following that the  damaged area has to be built up with matching filler conforming to the original deposit. You may use austenitic buffer layer, if the deposit requires multiple layers of build-up.

Hope the attached information would be of help.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFfyh2iqb2SdnB7bxvco3MZWzCPwHTfCHDxWHCAV-KS2fuaw9g%40mail.gmail.com.


Virus-free. www.avg.com
Guidelines for Weld Surfacing with ULTIMET® Wire.pdf
ultimet-extract.pdf
Reply all
Reply to author
Forward
0 new messages