PQT FOR A333 Gr.6 Material with PWHT

79 views
Skip to first unread message

Siva Chidambaram

unread,
Jul 15, 2015, 12:52:44 AM7/15/15
to material...@googlegroups.com
Hi,
 
I need to prepare WPS & PQT for the A333 Gr. 6 Material with PWHT as per ASME B31.3 with GTAW + SMAW process  & GTAW + FCAW.
Can anybody suggested what electrode shall I use for the process.
 
Thanks
M. Sivachidamabaram 

gupta...@yahoo.co.in

unread,
Jul 16, 2015, 2:27:38 AM7/16/15
to material...@googlegroups.com

You can use Gtaw &Smaw process ER 70 S2 & E 7018-1

A P Gupta
SIMAR
QC MANAGER

Sent from Yahoo Mail on Android



From: Siva Chidambaram <mechsivac...@gmail.com>;
To: <material...@googlegroups.com>;
Subject: [MW:23161] PQT FOR A333 Gr.6 Material with PWHT
Sent: Wed, Jul 15, 2015 4:26:41 AM

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMV4LCnpAL%2BEaywhFg6MiDpXkHATSKu_vF9z9xpOJgDefA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

joydev dalai

unread,
Jul 16, 2015, 2:29:41 AM7/16/15
to materials-welding

ER 807NI1 FOR ROOT AND HOT PASSES
FOR OTHER PASSES U CAN USED E7018 H4R


Regards,

Joydev Dalai
   

--