Dear Expert,
“X” welder working with company and left the organization. Again after Two or three year he is joining back same company. All earlier certificate is available with company with proper documentation.
Is it possible to renew his earlier certificate with one sample based on RT or visual inspection OR All new qualification is to be done New. Qualification code is ASME SEC IX.
Pls provide your valuable input with standard reference.
Thanks & Regards,
Mohd. Azam
Doha-Qatar
Subject: [MW:24008] Welder Qualification as per ASME SEC IX |
Dear you can check his continue progress record of earlier based on that will able to test with RT or bend test.
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/534889103.3167229.1451277057695.JavaMail.yahoo%40mail.yahoo.com.
| From: Bharat Kumar Sent: Παρασκευή, 1 Ιανουαρίου 2016 - 20:21 |
Reply To: material...@googlegroups.com |
Subject: Re: [MW:24028] Welder Qualification as per ASME SEC IX |
Get continuity records of welding carried out for that process and based on continuity u can extend his validity.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFPbJeYV6ZhijTfrqt9fp2viY4kSja%3Dx7nxVOe_WF7TZMLu1Nw%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFPbJeYV6ZhijTfrqt9fp2viY4kSja%3Dx7nxVOe_WF7TZMLu1Nw%40mail.gmail.com.
Hi Mohd. Azam,
Please look though the following extracts from Sec-IX. It’s advisable to test and qualify the welders separately and before assigning them in production joints.
Thanks..
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
All provided answer are personal opinions or personal judgements only. It's not connected with any employers by any means.
QG-106.3 Simultaneous Performance Qualifications.
(f) When the person changes employers between participating organizations, the employing organization shall verify the continuity of the person’s qualifications has been maintained by previous employers since his qualification date, as required by the applicable Part for the joining method. Evidence of activities supporting performance qualification continuity may be obtained from any member of the association, even if the member was not a participant in the simultaneous welder qualifications.
(g) If a person has had their performance qualification withdrawn for specific reasons, the employing organization shall notify all other participating organizations that the person’s qualification(s) has been revoked. The remaining participating organizations shall determine whether or not they will uphold or withdraw the performance qualifications for that person in accordance with this Section.
(h) When a person’s performance qualifications are renewed in accordance with the provisions of the applicable Part for the joining method, the testing procedures shall follow the rules of this paragraph. Each renewing organization shall be represented by an employee with designated responsibility for performance qualification.
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Rajagopal Kannan
Sent: Sunday, January 03, 2016
11:45 PM
To: material...@googlegroups.com
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD3oVpD15j%2BmGz1KSoHHF2Eh2ZV1qkypbam4DbgsF3xatNHnGg%40mail.gmail.com.
Suppose welder leave the co.and again join mid gap 6 month requalified of welder
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/wbnff1m8h1et9phx9alpoay8.1456917106343%40email.android.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC85Fd8Vc3Ex3NDTAhvTPnd_Nc%3DWPti-52nSt19eHhGoBSArSQ%40mail.gmail.com.
Get your own FREE website, FREE domain & FREE mobile app with Company email. | Know More > |