Dear Experts,
I would like to get your advice and opinion about the welding og above subject.
We have to weld 1000 shear anchors on stainless steel 10 mm thick
Following are the quality of the plate and anchor.
Plate SA 240 Type 304
Shear Anchor 16x150mm S235J2+ C470
I would like to know whether we use shear anchor welding machine to do the welding. These are the two different materials and chemical compositions are different we have to use SS 309l welding rods and do the manual welding using SMAW or FCAW welding process.
Please give your valuable opinion.
Thanks in advance.
Cyriac Dominic