Dear all experts,

 What is the temprature limitation (Max.& Min. ) to use for both A106 & A333?

Regards, 
Mahmood 

Vishwas Keskar

unread,
Nov 21, 2022, 5:17:58 AM11/21/22
to material...@googlegroups.com
What are service conditions ?
MDMT for both the materials ?


Sent from my iPhone

On 21-Nov-2022, at 3:33 PM, Mahmood Al-Hinai <hyna...@gmail.com> wrote:


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEuX%2BdkzQwXLqxkK7kecUMiNexGbyY3WnxeaB%2BYZ5cHmiKBAEA%40mail.gmail.com.

Mahmood Al-Hinai

unread,
Nov 21, 2022, 6:16:30 AM11/21/22
to material...@googlegroups.com

Vishwas Keskar

unread,
Nov 21, 2022, 10:29:02 PM11/21/22
to material...@googlegroups.com
Ok ,
What is the operating  service temperature of Water and Oil  in the said designed equipment / Piping 
?

Sent from my iPhone

On 21-Nov-2022, at 4:46 PM, Mahmood Al-Hinai <hyna...@gmail.com> wrote:



Mahmood Al-Hinai

unread,
Nov 22, 2022, 12:34:31 AM11/22/22
to material...@googlegroups.com
Design temperature up to 82 degree celsius.


Vishwas Keskar

unread,
Nov 22, 2022, 2:44:55 AM11/22/22
to material...@googlegroups.com
Ok 
Both SA 106 gr B and SA 333 Gr 6 can be used.
Discuss with Design  Engineering Manager

Sent from my iPhone