On 22-May-2023, at 8:40 AM, Mahmood Al-Hinai <hyna...@gmail.com> wrote:
Dear all experts,If Low Hydrogen Electrods kept directly in a holding oven without backing, and later on it was observed, so how to rectify?Shall be scraped or backed?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEuX%2Bd%3D-LvqWgQ-qVC0KqtfcVEP8_haQFEHEK%2BqSw87Ss8ms%3Dg%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F033F967-E354-40A3-A48C-628EBF34D5E9%40gmail.com.
Hi, Good day,
When it comes to baking, you need to maintain the backing oven temperature 260-430 degrees Celsius. While maintaining a temperature of 120 degrees Celsius is for holding purposes,. At 120 degrees Celsius, the flux coating does not experience any significant heat impact, which can’t potentially lead to flux damage, baking requires a higher range of 260-430 degrees Celsius.
Considering the above statement you can go for baking.