Dear All
 In our spec. a formula is coming to calculate percentage Strain for tubular section as follow: 
PS % = (t/D) x 100
Now how can calculate strain age for other sections such as HEB?because in certificate of HEB that attached the amount of impact test for unaged condition measured .
Regards.  

1. HEB 600 TAG# T1031 MANUFACTURER MTC.pdf

Rems Okonkwo

unread,
Mar 20, 2015, 11:51:10 PM3/20/15
to material...@googlegroups.com
Percentage of Strain is required for welded tubulars, it is required mainly dring codl rolling of plate to form tubular section to enable you ascertain the level of strain during cold rolling.
 
From the formulae, the higher thickness used for formming lower diameter will be subjected to higher strain than otherwise.
 
Percentage of strian is not required for rolled section such as HEB.
 
Regards,
 
Rems
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALcH7WDB2xxrw0DyxkrQNJ071Hi1LkgwoCkCZNtboNJ7KtfzTw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages