Dear Expert's,
           How we can differentiate CS materials and NACE materials when we stake cumulatively?
GA E-60021 what's this coding in the materials?
If it is a traceability means,is it mandatory on the materials?

Rems Okonkwo

unread,
Feb 11, 2015, 6:47:29 AM2/11/15
to material...@googlegroups.com
Dear Mr Vasan,
 
CS materials can also be use for NACE materials, the different will be on the material selection with respect to Chemical Composition and the level of testing as required in NACE M0175
 
Regards,
 
Rems Okonkwo
IWE Nigeria

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABMP0bNO_DU%2BiuexRXOe-4GD6%2B8dfdrgVb9WddKcGLchGcfR-A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Ritesh Rajput

unread,
Feb 11, 2015, 9:27:07 AM2/11/15
to material...@googlegroups.com
 Following two thing matches in the material as per NACE MR 0175, 

1. Sulphour  content <=0.010% 
2. Hardness Value  <=22 HRC
3. NACE Marking shall be require on material ( with Help of document also can certified)

Thank you very much 

best of regards

RItesh Rajput 


--