https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEkUWtJG62wA-s8TVHu1peHGwu%2B%2BROMNm0HwewBwQPym56reZg%40mail.gmail.com.
--
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEkUWtJG62wA-s8TVHu1peHGwu%2B%2BROMNm0HwewBwQPym56reZg%40mail.gmail.com.
Hello,
NDE(RT) and Hydrotest both having different purpose.
NDE are carried out to ensure the defect free joints and hydrotest is carried out for strength well as leak test.
NDE we are only doing at weld and their HAZ area. However before putting in the system complete piping system need to be tested.
Incase of golden/ closure weld where Hydrotest is not possible there 200 NDE shall be carried out but this is not applicable for all the joints.