Hi Mostafa,
These techniques are very specialized techniques. Not all NDE techs are up to speed with both of these techniques. Please see some guidelines from the BINDT on the same.
I’m not sure , where you’re located, you may check with the local high profile NDE Schools or Companies, who’ll have those personnel in their team
Thanks.
Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist &
Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAI6C/nhitp9NlnqAyYQt%2BycBAAAAAA%3D%3D%40quickclic.net.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1141766489.4415183.1455694544189.JavaMail.yahoo%40mail.yahoo.com.
As I understand PAUT & TOFD are NDE UT technics and not NDE methods. Hence NDE Level III in UT is required with training in special technics.
Regards
P. V. Ghanekar
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAI6C/nhitp9NlnqAyYQt%2BycBAAAAAA%3D%3D%40quickclic.net.