Hope all member will be fine,
I have a many question about RT,
1. What we can use RT level on Tank?
2. Reference of RT level in ASME Section VIII Div-I ? or any other reference standard (API/ASME) except Section V. 
3. If tank design by API Standard, can we use ASME VIII Div-I reference for RT?
4. If weld length of but weld joint is 32 mtr, as per RT-3, how much 6" film are required as per code.  

Please guide me in short and proper words that we can under stand.

Best Regards

Regards,

GMT

Save life| Don't destroy nature | Help save paper

Andrew Ubakwem

unread,
Sep 7, 2020, 6:45:51 AM9/7/20
to material...@googlegroups.com
Dear Ghulum,

I seems not to understand your query because either your English composition is confusing me the more or I do not get basis for your questions.

Question#4: weld length 32mtr? 

Please clarify.

Regards,

Andrew.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3561e869-1bdd-4112-bf46-b0e86b82f936n%40googlegroups.com.

james gerald

unread,
Sep 7, 2020, 6:57:08 AM9/7/20
to material...@googlegroups.com
Specify your Design code as RT-3 is applicable only for Pressure vessels fabricated of ASME Sec VIII 

Thanks & Regards

J.Gerald Jayakumar




Ghulam Mustafa

unread,
Sep 8, 2020, 12:41:33 AM9/8/20
to material...@googlegroups.com
Dear all,
hope all members are fine, 
Our company is fabricating a Mud Tank. the client requirement that RT-3 will be performed. I want only one question: how much RT film is used in this tank if the total weld length is 32 meter and its RT reference code for satisfying the client.

this tank as per API standard.
and reference will be API.


guru vasanth

unread,
Sep 8, 2020, 1:31:49 AM9/8/20
to material...@googlegroups.com
Gulam

First you read the design code .and it will give RT requirement and acceptance reference code details .

Regards 

Guru S

செவ்., 8 செப்., 2020, முற்பகல் 10:11 அன்று Ghulam Mustafa <gmt...@gmail.com> எழுதியது:
--
Thanks and regards Guru.s.m

George Dilintas

unread,
Sep 10, 2020, 8:49:25 AM9/10/20
to material...@googlegroups.com
ASME BPVC Section VIII Div. 1 requirements do not apply to tanks. Tanks are covered by API codes (650, 620).
In case you have a pressure vessel and RT 3 is required you have to perform spot radiography in all Category A & D butt welds (see fig. UW-3) of type 1 & 2 (see UW-12).
Then you have to perform also spot RT in Category B and C butt welds when they intersect Category A welds.
For more details, you have to read UW-11


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3561e869-1bdd-4112-bf46-b0e86b82f936n%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages