Weld Details of Tanks.

41 views
Skip to first unread message

Ashishranjan - Domech Fabricators Pvt.Ltd.

unread,
Aug 22, 2025, 7:55:22 AMAug 22
to material...@googlegroups.com
Dear team 

What is the difference between these two weld details??? 
And what about your comment on back chip 
Of these joints required or not. 

Regards,

Ashish Ranjan

Go green logo

Save a tree...Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hardcopy.



"Confidentiality Warning: This message and any attachments are intended only for the use of the intended recipient(s), are confidential and may be privileged. If you are not the intended recipient, you are hereby notified that any review, re-transmission, conversion to hard copy, copying, circulation or other use of this message and any attachments is strictly prohibited. If you are not the intended recipient, please notify the sender immediately by return email and delete this message and any attachments from your system.

Virus Warning: Although the company has taken reasonable precautions to ensure no viruses are present in this email. The company cannot accept responsibility for any loss or damage arising from the use of this email or attachment."


Caution: The e-mail below is from an external source. Please do not open attachments or click links unless this email comes from a known sender and you know the content is safe.

1000545962.jpg
1000545961.jpg

kumar sumit

unread,
Aug 23, 2025, 4:31:31 AMAug 23
to material...@googlegroups.com
Dear Ashish
In the picture share by you that is longitudinal/Vertical seam which shown the double grove that means if the Welding completed from outside backchip is required from other side(inside).

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BRvhZCyYaqU8tXrgeL_2AxM5eR0XDZ7mkeB6krre%3DVKgUO0bQ%40mail.gmail.com.

Ashishranjan - Domech Fabricators Pvt.Ltd.

unread,
Aug 23, 2025, 10:36:47 AMAug 23
to material...@googlegroups.com
Thanks Sumit for response. 

But my question is i have attached two weld pictures. In one pictures it clear that double v shows in that back chip we do from inside but what about the single side pictures back chip required or not.

Regards,

Ashish Ranjan

Go green logo

Save a tree...Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hardcopy.



"Confidentiality Warning: This message and any attachments are intended only for the use of the intended recipient(s), are confidential and may be privileged. If you are not the intended recipient, you are hereby notified that any review, re-transmission, conversion to hard copy, copying, circulation or other use of this message and any attachments is strictly prohibited. If you are not the intended recipient, please notify the sender immediately by return email and delete this message and any attachments from your system.

Virus Warning: Although the company has taken reasonable precautions to ensure no viruses are present in this email. The company cannot accept responsibility for any loss or damage arising from the use of this email or attachment."


Caution: The e-mail below is from an external source. Please do not open attachments or click links unless this email comes from a known sender and you know the content is safe.

venkateswara reddy Desireddy

unread,
Aug 23, 2025, 12:29:38 PMAug 23
to material...@googlegroups.com
For single V groove not required back chiping if root weld done with TIG process. If SMAW process used for root weld, then back chip need because of penetration and slag issues.