Welder Qualification as per ASME SEC IX E6010-E7018

66 views
Skip to first unread message

ROLANDO RC

unread,
Apr 6, 2025, 9:19:28 AM4/6/25
to Materials & Welding
Good morning, group. I'm asking for your help with the following topic: ASME IX Welder qualification:
- 3" Sch 80 pipe - SMAW E6010 (t: 2.62 mm) - SMAW E7018 (t: 5 mm) What is the qualification range for F3 and F4?
Regards

venkateswara reddy Desireddy

unread,
Apr 7, 2025, 12:29:03 AM4/7/25
to material...@googlegroups.com
Two times of the deposit material thickness.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1d3d6208-ab11-4466-8074-b06af7932050n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages