Dissimilar chemical composition weld

110 views
Skip to first unread message

Sintha Aidroos

unread,
May 22, 2023, 10:57:12 PM5/22/23
to material...@googlegroups.com
Dear experts,
                Please advise about weld metal deposit  composition for base metal cuni 90/10 (UNS C 70600) and filler wire CuNi70/30 (UNS C 71500) combination of this material.We checked PMI at weld joint area but composition is not matching with ASME sec II part C .Can you give guidance for any PMI acceptance criteria?Here I attached PMI report for your review.

As per ASME sec II filler metal nickel percentage is 29-32 % and copper remaining.


 Regards

Aidroos      

RANEESH PK

unread,
May 22, 2023, 11:22:56 PM5/22/23
to material...@googlegroups.com

Hi,

1. Alloys are acceplable if the alloying elements are each within 10% of the specifled range of values. 


2. Welds with consumables that match, or nearly match, the base meal composilion shall be within +12.5% of the ranges allowed in ASME SEC IIC for each element.Chemical Composition of Material specs must be verifled/avallable.

thank you 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM11Z9UL_Wt3U7Rzr06B1XsBxQwmXYeSDsUp6seDEc1%3DOmNAfg%40mail.gmail.com.

Parminder Singh

unread,
May 24, 2023, 7:31:26 AM5/24/23
to material...@googlegroups.com
Hi, 

Please refer ASME Sec I Non Mandatory Appendix - B Clause B-8

Thanks 
Parminder Singh

--