Dear

I have a question about my Inspection Certificate of pipe fitting.
We order of material for low temperature ASTM A420 Gr. WPL6.
But, in hard stamp and certificate is "WPL6/WPB" (Attached)
Where i know, for WPB is ASTM A234.
what is the product can used for Low Temperature Service -45degree Celcius???
and if true, any one know reference from standard ASTM???
MTC of Benkan WPL6 WPB.PDF

anand gupta

unread,
Jul 6, 2019, 10:47:43 AM7/6/19
to material...@googlegroups.com, Sulfi Afdhal
WPB is for high temp and WPL6  is for low temp. 
You can not use. 

Regards 

A p gupta 
ThyssenKrupp 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4d83d7bf-10a1-4d0e-8cb7-6a0efd0c7679%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

anand gupta

unread,
Jul 6, 2019, 10:47:43 AM7/6/19
to sulfi...@gmail.com, material...@googlegroups.com
I think it was punch by mistake. 
No body manufacturer one product with dual spec. 

Regards 
A p gupta 
ThyssenKrupp 
On Sat, 6 Jul 2019 at 9:20, U2L Poenya

Thank’s for your advice sir..

But, why the manufacture make the product with double spec in same of part

 

Thanks

 

 

SuLfi

 

Sent from Mail for Windows 10

Dinesh Somwanshi

unread,
Jul 7, 2019, 11:16:54 PM7/7/19
to material...@googlegroups.com, sulfi...@gmail.com
Dear dual product may possible if follow & meeting criteria. 

Please review MTC. 

Regards

Dinesh

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


--
Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
 00919881344135 India 
Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


Dindo

unread,
Jul 9, 2019, 12:54:43 AM7/9/19
to material...@googlegroups.com
The fittings are dual certified, you can use them for both classification.