Dear All,Can any one please clarify whether what NDT procedure should follow regarding welding of cleats in supports for pressure vessel.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BsNR02W3rUEE1PbuGeSEkc25iv8ii5-FJuuL1%2B5hT4O--%3Dwsw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrWr%3DScSqQN0DHdWAz3XcfqQeKH0sH9jDt5D85iWhX9-rA%40mail.gmail.com.
Dear Sir.
The cleat is temporary for fabrication right ? Is anything you were noticed in Project specs?
However after temporary cleat removal, PT - MPTon pipe affected area is recommend.
Thanking You,
With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BsNR03YSeE7sT0Gjt%2Bkq-D9DGowtrQztW28ynWAybxeNX4j6A%40mail.gmail.com.