Skip to first unread message

Sfmech

unread,
Jan 24, 2020, 10:57:29 PM1/24/20
to Materials & Welding
Hello, is there any method to find weight of scrap electrodes, approximately. The electrodes are 6013 and are placed in a heap.

Dinesh Somwanshi

unread,
Jan 25, 2020, 12:41:36 AM1/25/20
to materials-welding
Dear, 


Calculate the weight of entire electrode.

calculate weight stubborn electrode .

Deduction of both multiplied number of electrodes will give correct answer.

Regards

Dinesh

On Sat, Jan 25, 2020, 09:27 Sfmech <sharje...@gmail.com> wrote:
Hello, is there any method to find weight of scrap electrodes, approximately. The electrodes are 6013 and are placed in a heap.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d1bca86c-aef6-4e98-aa3a-822914ac1829%40googlegroups.com.

Kiran PTN

unread,
Jan 25, 2020, 4:51:45 AM1/25/20
to material...@googlegroups.com
Hi,

Efficiency of SMAW process is ~ 60-65%
Hence multiply the E6013 quantities (Kg) procured/ consumed by 0.4, to arrive at apprx wastage qty.

Regards,
Kiran