What is the meaning of oscillation(ASME sec IX, QW-410.7) in automatic welding??

Regards,
Aby

Dinesh Somwanshi

unread,
Apr 17, 2017, 3:53:16 AM4/17/17
to materials-welding
dear sir

oscillation: for a machine or automatic process, an alternating motion relative to the direction of travel of welding, brazing, or thermal spray device. 

As per ASME 9. pAGE 9.

rEGARDS

dINESH


*DINESH VITTHAL SOMWANSHI*

*BACHELOR IN MECHANICAL ENGINEER*

*AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL,*
*API 570 - Piping Inspector,** AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3*
*NDT II -UT , RT , MT , PT, VT*
00919881344135
Skype = dinesh570_1

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACdTRdzpg97tBwZ_ovjDZ_9_A%2Bk1xtHYaxhPfQj6OS-QA7vF%3Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Prakash Hegde

unread,
Apr 17, 2017, 11:45:27 PM4/17/17
to material...@googlegroups.com
 Oscilation : applicable to Machine/Automatic welding system where welding is being carried with programed movement of welding torch i.e. you can pre set movement in x, direction ,also  movement distance  of torch/arc  and this is fixed once welding starts viz, from right to left or vice versa 
While as weaving during welding is generally for manual welding and this is being controlled by welder it depends upon the position ,Weld joint configuration etc and this is variable  and weld properties depends upon weaving size , particularly Impact properties

Regards
Hegde


To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrUBYMy3acbuRv0W1k4rN8wYCq4nED5scRA1j8HYBsKeFQ%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages