Dear sir,
Please provide highlighed details for the welding of 2 mm GI sheet
welding with GMAW SOLID WIRE 70SX welding process.
As found on fillet joint i have tried with faying surface cleaning
prior to weld still found pores in joint.
Please advice.
--