In welding procedure qualification as per API 1104, does Butt Weld qualification also qualifies branch and fillet welds?.

Regards,

Thulaib

Mostafa DAIF

olvasatlan,
2024. márc. 30. 20:41:56márc. 30.
– material...@googlegroups.com
Dear all,

In the context of welding procedure qualification outlined by API 1104, it’s important to note that the qualification of a butt weld does not extend automatically to branch and fillet welds. Each type of weld necessitates its own distinct qualification procedure.

Best regards,


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JMkVLyYtdx0p-Pyuni4xchxmqY9QKjBT1D-syjF23V4mg%40mail.gmail.com.

Ramamoorthi Thangarasu

olvasatlan,
2024. márc. 31. 10:11:50márc. 31.
– material...@googlegroups.com
Hi
API 1104 given Direction if any changes for welding Parameters  need new WPS...Below and Over12 inch dia & Thickness. 
WQT also....


madheswaran s

olvasatlan,
2024. ápr. 7. 11:51:38ápr. 7.
– material...@googlegroups.com
Dear all,, But weld qualifies Fillet weld as per API 1104 ,but not vice versa.