Plug Welding

65 views
Skip to first unread message

Ashish Chacko

unread,
Oct 24, 2023, 9:12:57 AM10/24/23
to Materials & Welding
I have a question regarding the use of a groove weld WPS for plugging a tube in an exchanger and whether it is necessary to qualify a Tube-to-Tubesheet (TTS) WPS instead. I would greatly appreciate your insights on this matter.

As per my understanding since it is a fillet weld we can do. If not please provide me reference.

bavithran samuthralingam

unread,
Oct 24, 2023, 12:01:36 PM10/24/23
to material...@googlegroups.com
Groove weld WPS cannot be used in tube to tube sheet welding in heat exchanger Tube replacement . Separate WPS need to be prepared as per ASME SEC 9 and also the welder need to be qualified using that WPS 

On Tue, 24 Oct 2023 at 4:12 PM Ashish Chacko <iamash...@gmail.com> wrote:
I have a question regarding the use of a groove weld WPS for plugging a tube in an exchanger and whether it is necessary to qualify a Tube-to-Tubesheet (TTS) WPS instead. I would greatly appreciate your insights on this matter.

As per my understanding since it is a fillet weld we can do. If not please provide me reference.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0554da58-cb54-469e-b60d-1210621da32en%40googlegroups.com.

Vishwas Keskar

unread,
Oct 24, 2023, 12:01:36 PM10/24/23
to material...@googlegroups.com
Ashish 
You can use the groove qualified WPS 
Enure ASME sec IX requirements are met 
Essential ,Non essential ,Supplentary  variables 
Thanks 
Vishwas IWE 
Sent from my iPhone

On 24-Oct-2023, at 6:42 PM, Ashish Chacko <iamash...@gmail.com> wrote:

 I have a question regarding the use of a groove weld WPS for plugging a tube in an exchanger and whether it is necessary to qualify a Tube-to-Tubesheet (TTS) WPS instead. I would greatly appreciate your insights on this matter.


As per my understanding since it is a fillet weld we can do. If not please provide me reference.

--

Ramamoorthi Thangarasu

unread,
Oct 24, 2023, 12:01:48 PM10/24/23
to material...@googlegroups.com
Hi

If WPS Qualified for Groove welds also qualified for fillet weld only want to check for thickness rank for approved WPS.

Regards
Ramamoorthi Thangarasu

On Tue, Oct 24, 2023 at 6:42 PM Ashish Chacko <iamash...@gmail.com> wrote:
I have a question regarding the use of a groove weld WPS for plugging a tube in an exchanger and whether it is necessary to qualify a Tube-to-Tubesheet (TTS) WPS instead. I would greatly appreciate your insights on this matter.

As per my understanding since it is a fillet weld we can do. If not please provide me reference.

--

bavithran samuthralingam

unread,
Oct 26, 2023, 2:32:14 AM10/26/23
to material...@googlegroups.com
Hi 
For this tube to tube sheet welding separate wps need to be prepared and the welder should be qualified with that wps 
Kindly refer QW-193 in ASME SEC IX 😊😊