FILLER WIRE

350 views
Skip to first unread message

SIKANDAR SHARMA

unread,
Dec 25, 2023, 10:51:54 AM12/25/23
to Materials & Welding
Dear Sir

Can any one suggest me, which GRADE filler matel used for is2062 E350 BR  ms material

ASME  sec ix  SMAW WPS ,PQR


Thanks 
Sikandar Sharma




Mohd Siraj

unread,
Feb 23, 2024, 3:11:54 AM2/23/24
to Materials & Welding
AWS A5.1 E7018 or equivalent.

Ramamoorthi Thangarasu

unread,
Feb 25, 2024, 1:47:57 AM2/25/24
to material...@googlegroups.com
If you want to use different welding process , ER70S & ET70-1,,But need SMAW then you want to conform your parent material tensile strength based on this you can select 6018 or 8018 ......etc

On Fri, Feb 23, 2024 at 11:11 AM Mohd Siraj <mohd...@gmail.com> wrote:
AWS A5.1 E7018 or equivalent.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5f8647ae-934e-4e2f-9f75-1adaa7e56857n%40googlegroups.com.

Srinivas Rao

unread,
Feb 25, 2024, 5:30:09 AM2/25/24
to Materials & Welding
for single side full penetration welds : 
GTAW/GMAW- ER70S6 /ER 70S2 
SMAW : E7018 OR E7018-1 
FCAW : E70T-1
SAW: EM12K 

Thanks & regards,
Srinivas Rao