Rivetted like object in piping

7 views
Skip to first unread message

Pradeep kumar hormis

unread,
Jul 26, 2015, 10:43:30 AM7/26/15
to material...@googlegroups.com
Dear Experts
 
Is any body experienced with indication on piping with attached pictures. I observed it in 48 " carbon steel piping.
 
please advice
Thanks & Regards

PRADEEPKUMAR HORMIS


 
 


 
IMG-20150721-WA0143.jpg