Dear all,

Can we use low Hydrogen Electrode in under ground pipeline works.??
If yes , please let me know standards and clause.

From
Herish

MADHUSOODHANAN NAIR .G

unread,
Apr 28, 2020, 8:04:20 AM4/28/20
to material...@googlegroups.com
Dear Harish Varude 


      As per the API 1104 (Welding of pipelines and related facilities) clause 4.2.2.1 & 5.4.2.7 is addressing the usage of low hydrogen electrode so you can use LHE for underground pipelines.LHE were developed for welding low-alloy, high-strength steels.
Regards
Madhusoodhanan Nair.G
Sr Manager (Operations)
VCS Quality Services Pvt Ltd

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKK3Do52gdMLiUL9Ub%2BbRXBGz3%3DmLZYd_W7wJeEjh3Q61Q%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages