IMPACT EXEMPTION FOR DUPLEX FLANGES SA 182 Gr F51

176 views
Skip to first unread message

VISHNU

unread,
Dec 24, 2015, 4:14:52 AM12/24/15
to Materials & Welding
Dear sir,

I have one query regarding to above subject,

One of the definition of governing thk when using fig. UCS-66 - Governing thickness of flat non welded parts, such as bolted flanges, tubesheet and flat head is the flat component thickness divided by 4

But what about Duplex flanges ? UHA is not giving such clause, so what will be governing thickness to be consider for duplex flanges (SA 182 F51) ?

Thanks in advance

Regards

vishnu 

Raghuram Bathula

unread,
Dec 24, 2015, 4:28:57 AM12/24/15
to Materials-Welding
i guess you should use Appendix JJ, 
UHA -51(g)?

Vish

unread,
Dec 28, 2015, 2:29:30 AM12/28/15
to Materials & Welding
Thanks MW,

But my question remains same that, what will be nominal thickness of duplex flanges to be consider ?
 

vish

Mehdi Vafakhah

unread,
Dec 29, 2015, 10:21:07 PM12/29/15
to Materials & Welding
Dear vish


In UCS-66 the governing thickness is important factor cause we have combination of minimum design metal temperature
 and governing thickness to the subject material. 

but in UHA-51 impact test requirement is based on the material properties and material thickness is not an essential variable . (except where noted)

UHA-51 IMPACT TESTS
Impact tests, as prescribed in (a),shall be performed
on materials listed in Table UHA-23 for all combinations
of materials and minimum design metal temperatures
(MDMTs) except as exempted in (d), (e), (f), (g), (h),or
(i). 


Best regards.

-------------------------------