Dear All,
Need your guidance on subjected topic.
I need filler which will be use to weld X2CrNiN18-7 material (equivalent ASTM material 301NL (Which has 550 MPa minimum tensile requirement).
Generally we use ER 308L material to weld this material but as per EN 10088-2, we need minimum tensile value 650MPa.
Tensile value for Filler wire- ER 308L is 520MPa minimum.
We have some PQR which is less than 650 MPA, so it can not be use.
I checked Filler wire MTC which has 610 MPa tensile value (less than requirement).
So which filler wire can be suitable to weld this material.
Please provide your valuable reply.
Thank you
Vijay Katkar