CODE CASE 2945: AN EXTENSION FOR QUALIFICATION OF IMPACT-TESTED WELDED PROCEDURES
94 views
Skip to first unread message
Raghuram Bathula
unread,
Aug 28, 2019, 12:06:45 AM8/28/19
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials-Welding
2017 editions of ASME Section VIII-1 and Section VIII-2 has new requirements for the qualification of impact-tested weld procedures, found in ASME Section VIII-1, subparagraph UG-84(h)(5), and in ASME Section VIII-2, subparagraph 3.11.8.3(g), introduced restrictive requirements for the removal of impact test specimens when multiple weld processes are used.
Code Case 2945 give some relief to fabricators to use previous qualified procedures provided
(a) The welding procedure specification was qualified prior to January 1, 2018, and the procedure met the requirements of the Section VIII, Division 1 and Division 2, 2015 Edition.
(b) The existing welding procedure specification may be used until the 2021 Edition of Section VIII, Division 1 and Division 2 go into effect on January 1, 2022.
extension applies only to non-compliance with the specific new requirements that it mentions, and will not automatically apply to any other new requirements introduced in the 2019 editions of these codes.